Spark spectral analysis of low-alloy and unalloyed steels

We offer resilient material analyses including the necessary sample preparation by cutting and grinding your samples. The test reports contain a representation of the elements determined with details of the contents in mass%. A comparison with the target composition or comparison materials as well as a conformity statement with details of a material number can also be made.

Determination of elemental composition. Accredited for the following concentration ranges (in mass %)

 

Element Min Max
carbon 1,9 3,8
Chromium 0,025 2
Copper 0,015 0,75
molybdenum 0,01 1,2
Manganese 0,03 1,8
Nickel 0,02 2
Phosphorus 0 0,4
silicon 0,15 2,5
sulfur 0,01 0,08
tin 0,004 0,12
vanadium 0,008 0,22